Blog · November 12, 2026

Inlet Pressure in PU Metering Pumps: Symptoms and Checks

A polyurethane metering pump delivers short shots at high output, the ratio drifts by a fraction of a point, and the first suspicion falls on the mixing head, the valves or the pump itself. The suction side rarely gets checked because it usually has no gauge. Inlet pressure is the condition that decides whether each pump cavity fills before it discharges, and a positive-displacement pump cannot deliver volume that did not enter the cavity first. The mechanics hold across machine types and sizes: how inlet pressure is created, why starvation, cavitation and air ingress produce different symptoms, and which measurements separate a suction problem from a worn pump before anyone rebuilds hardware.

Why Inlet Pressure Decides What a Metering Pump Actually Delivers

Gear pumps, piston pumps and screw pumps share one behavior. Each revolution or stroke displaces a fixed geometric volume. Outlet flow is that volume multiplied by shaft speed and by volumetric efficiency. When volumetric efficiency falls, nothing on the machine reports it. The shot still completes, the timer still runs, and the part leaves the mold lighter than the recipe intended.

Volumetric efficiency drops for two separate reasons. Internal slip returns material past the pump clearances, and slip rises with the pressure difference between outlet and inlet. Incomplete fill leaves part of the cavity empty, and fill depends on the pressure available at the inlet and the time available before the cavity closes. Slip is a pressure-ratio problem. Fill is a suction problem. Inlet pressure governs the second one, and it is the variable most machines never measure.

On a two-component machine the result is not a simple output loss. If the polyol pump loses fill while the isocyanate pump holds its volume, the mixing ratio moves by roughly the same percentage as the loss. Density, hardness, cream time and demold behavior follow the ratio, so the first visible sign is often a part that is soft, heavy or slow to set rather than a part that is visibly short.

In a 2K PU machine the metering pumps sit between the day tanks and the mixing head. Everything upstream of the pump inlet is suction; everything downstream is pressure. Most maintenance attention goes downstream, because that is where the gauges, the valves and the mixing head are.

The layout of a 2K machine explains why suction faults are so often misread. <How Polyurethane Foam Machines Work: Types and Applications> covers how the metering, mixing and control sections connect across different polyurethane foam machine types.

a1

Where Inlet Pressure Actually Comes From

At the pump inlet, the pressure available is the tank pressure plus the static head of material above the pump, minus the losses in the suction line:

p_inlet = p_tank + ρ g h − Δp_line

On a vented day tank, p_tank is atmospheric and largely cancels against ambient pressure at the pump seal, so the working number is static head minus line loss.

Static head depends on density, on gravity, and on the height h measured from the pump inlet centerline to the liquid surface at the minimum working level, not at the full level. A day tank that runs from nearly full to nearly empty changes that height across a shift, and a machine that meters cleanly at the start of a run can drift at the end of it.

Line loss is where most of the surprises sit. Polyol and high-viscosity isocyanate move through suction lines in the laminar range, and in that range pressure drop rises with viscosity, with line length, with flow, and with the inverse fourth power of the internal diameter. One size up in suction hose does more for inlet pressure than almost any other single change, while an added elbow or a reducing bush at the pump inlet gives part of that gain back.

The conventional way to state the requirement is net positive suction head available at the pump inlet, (p_tank − p_vapor)/(ρ g) + h − h_loss, held above the head the pump needs. A positive-displacement metering pump tolerates a thinner suction margin than a centrifugal pump of the same flow, which is exactly why the fault stays hidden until speed or viscosity rises.

Factor Effect at the pump inlet What to check
Day tank level and mounting height Sets static head, which falls as the tank empties Height from pump inlet centerline to liquid surface at minimum working level
Suction line diameter and length Laminar friction scales with length and the inverse fourth power of diameter Line bore against the pump connection, total length, number of bends
Strainer condition Blockage adds pressure drop that appears only while material is moving Differential across the strainer during a shot, not at standstill
Material temperature and viscosity Colder material fills the cavity more slowly and raises line friction Temperature at the day tank and again at the pump inlet
Dissolved gas and entrained air Gas leaves solution when local pressure drops, and air enters through leaking joints Transparent section in the suction line, foam layer in the tank
Recirculation return routing A return discharging above the liquid level aerates tank and suction stream Return outlet position relative to liquid surface and suction point

a6

Starvation, Cavitation and Aeration Are Three Different Faults

Maintenance conversations use these three words interchangeably, and the confusion costs time because the corrections differ.

Starvation is a filling failure. The cavity does not take in enough material before it closes, no gas phase is involved, and the pump sounds close to normal or slightly rough. Delivery falls as speed rises, and an inlet gauge reads low while the pump is working.

Cavitation is a pressure failure. Local pressure at the inlet or inside the cavity drops below the vapor pressure of a component, or below the pressure that keeps dissolved gas in solution. Bubbles form and collapse on the discharge side, which produces knocking, needle flutter on the gauge and, over months, erosion of gear faces or piston check valves. The material does not need to be hot to cavitate; polyol carries dissolved air, and a restriction at the inlet is enough to release it.

Aeration is an ingress failure. Air enters from outside through a leaking flange, a porous or cracked hose, a suction line running partly empty, or a return that discharges above the liquid surface. Those bubbles do not dissolve again. They travel through the pump and the mixing head and end up in the part as voids, streaks or density variation.

The corrective direction differs for each. Starvation responds to more static head, a larger suction bore, warmer material inside its process band, or lower pump speed. Cavitation responds to a wider margin between inlet pressure and vapor pressure. Aeration responds to sealing the suction path, not to changing the pump.

Symptom Most likely mechanism Check that distinguishes it
Delivery falls as pump speed rises and recovers at low speed Starvation, cavity not filling in time Compare delivered mass per revolution at low and high speed
Knocking or crackling at the pump head, unstable gauge needle Cavitation from low local pressure Raise the day tank level or cut speed briefly; noise that stops at once points to suction pressure
Bubbles in a transparent suction section, foam layer in the tank Aeration from a leaking joint or a return above liquid level Pressure-hold the suction line with the pump stopped and the inlet isolated
Ratio drifts after a material lot change, pumps sound normal Viscosity or temperature shift, not a pump fault Log material temperature and shot mass against the process band
Drift on one component only, worse as discharge pressure rises Internal slip or pump wear Hold speed constant and raise mixing head back pressure
Short first shot after a standstill Drain-back, lost static head, or cold material in the line Check whether the suction line stays full and heated during idle

a9

Why the Problem Appears at High Output or After a Material Change

Cavity fill is time-dependent. Doubling pump speed halves the time available for material to enter, so a suction line that is marginal at half output fails at full output. This is the most common reason a line runs clean for months and then starts drifting after a capacity increase or a speed change in the recipe.

Temperature is a two-sided variable. Warming polyol lowers viscosity, which shortens fill time and reduces line friction. It also raises vapor pressure and lowers gas solubility, which narrows the margin against cavitation. Raising a day tank temperature to make a thick material flow can convert a starvation problem into a cavitation problem without changing the delivery numbers much. Hold the material inside the temperature band its technical data sheet specifies and correct the suction line instead.

Filled systems change the suction load. Calcium carbonate, glass bead and pigment paste raise viscosity and density, settle in slow sections of the line, and load the strainer faster. A filled polyol that metered well on a short direct stub can starve on a longer run with three bends.

Formulation and ratio changes move the flow split. A new recipe can give the polyol pump a larger share of total volume, and the pump with the weaker suction line is then the one carrying more material at the same speed.

Lot-to-lot variation and ambient conditions finish the job. Two deliveries of the same grade can differ in viscosity, and a machine commissioned in summer on warm material may struggle in a cold store. Commissioning data recorded at one temperature and one lot is not a proven operating window.

Process parameters that look acceptable at commissioning can sit outside the limit once speed and viscosity move. <Low Pressure PU Foam Injection Machine for Custom Molding: Process & Parameters> covers the process and parameter side of low-pressure PU molding for custom parts.

a14

Readings That Mislead and Checks That Separate Suction from Wear

Gauge location decides what a reading means. A gauge on the day tank headspace measures pad gas pressure. A gauge on the discharge measures mixing head back pressure. A gauge at the pump inlet, downstream of the last strainer and close to the pump, is the one that describes fill. A static reading taken at standstill shows static head and says almost nothing about a shot.

Two conclusions are unsafe on their own. A steady inlet gauge does not prove the cavity fills at maximum speed, because a gauge cannot see fill time. A low reading does not prove the pump is worn, because a restricted strainer or a collapsing hose produces the same number.

The checks below separate the causes with measurements rather than opinions.

  1. Fit an inlet gauge downstream of the last strainer and close to the pump. Record the static value and the value during a shot at low and at high speed.
  2. Measure delivered mass instead of reading the gauge. Use the machine calibration mode to dispense each component separately for a timed interval, weigh it, and compare against geometric displacement multiplied by speed. Weigh isocyanate in a sealed cup and follow the site handling rules.
  3. Run a speed test at constant temperature and back pressure. If delivery per revolution falls as speed rises, the cavity is not filling.
  4. Run a back-pressure test at constant speed. If delivery falls as mixing head pressure rises, the loss is slip, which points to pump clearances rather than the suction line.
  5. Verify static head at the minimum working level, not the full tank, and confirm the height against the pump inlet centerline.
  6. Inspect the suction path while material is moving: strainer differential, hose collapse, sharp bends, and any reducing bush at the pump inlet.
  7. Pressure-hold the suction line with the pump stopped and the inlet isolated. A gauge that falls, or bubbles that return at a joint, indicates air ingress.
  8. Check the tank: return line discharging below the surface, agitator speed low enough to avoid a vortex, and no foam layer carried into the suction.

How to Specify Inlet Conditions Before the Machine Is Built

Inlet pressure is easier to design than to repair. Write these values into the machine specification and the pump can be sized against a defined suction condition.

  • Viscosity range at process temperature for both components, including lot-to-lot tolerance.
  • Process temperature band, and how tanks, lines and the pump are heated and controlled.
  • Minimum and maximum day tank level, with the height of the pump inlet centerline below the minimum level.
  • Suction line bore, length, bends, and whether it is heated or insulated.
  • Strainer mesh and differential pressure indication.
  • Recirculation arrangement, including where the return discharges.
  • Pump type, displacement, and the maximum speed at which the required flow is reached.
  • Expected discharge pressure range at the mixing head.

A metering accuracy figure describes what a pump can hold when the inlet is fed properly. Haifeng specifies the LJJ series low-pressure foaming machine at ±0.5% metering accuracy, and the HF-LPM servo closed-loop metering system compensates flow error inside the metering loop. Neither corrects a cavity that a starved suction line left empty, because closed-loop control adjusts the command, not the fill. That distinction belongs in a factory acceptance test: run the machine at maximum speed, at minimum tank level, with the production material, and record delivered mass per revolution.

a17

Bring the Suction Side Into Your Next Machine Specification

Send the suction-side data before the pump is sized: viscosity and process temperature for each component, minimum tank level relative to the pump centerline, suction line bore and length, strainer mesh, required flow and mixing ratio, and the discharge pressure at the mixing head. Our engineers will check the suction margin and come back with a line size, tank height or a speed limit that matches your material.

Email info@haifeng-automation.cn or message WhatsApp 86 13566296633 with those values and the machine type you are working on.

FAQ

What inlet pressure should a polyurethane metering pump see?

No single number fits every material. State the requirement as a margin: enough pressure at the pump inlet, measured while the pump is delivering, to fill each cavity at maximum speed before the cavity closes, with vapor pressure and gas release pressure still below that value. In practice this means flooded suction with the minimum tank level above the pump inlet, a suction bore sized for low velocity, and confirmation by measuring delivered mass per revolution at maximum speed. A reading taken at standstill describes static head only and proves nothing about fill.

Can polyol cavitate in a metering pump if it is not boiling?

Yes. In PU metering, cavitation is usually gas release rather than boiling. Polyol carries dissolved air, and any restriction that drops local pressure, such as a partly closed valve, a fine strainer, a collapsed hose or a high suction lift, releases that air as bubbles that collapse on the discharge side. The signs are knocking at the pump head, needle flutter on the inlet gauge and a delivery loss that appears without any recipe change. Raising the margin, rather than venting the pump repeatedly, is the correction.

Does raising inlet pressure improve metering accuracy?

Only until the cavity fills completely. After that point the pump is already full, and extra inlet pressure adds seal load, hose stress and a stronger jet from the recirculation return, which can aerate the tank and make ratio stability worse. Raise the head or increase the line size when a speed or delivery test shows incomplete fill. If delivery per revolution is steady across the speed range, the suction side is not the constraint and the accuracy problem sits elsewhere.

Why does the ratio drift only when the machine runs near maximum output?

Because fill time shrinks as speed rises. At half speed the cavity has time to fill even with a marginal suction line, and at high speed it does not. If only one pump is affected, the mixing ratio moves by the percentage of that loss. Run a speed test at constant temperature: delivery per revolution that falls with speed points to the suction line or material temperature, while delivery that falls with back pressure points to pump wear.

If you’re interested, check out these related articles:

How Polyurethane Foam Machines Work: Types and Applications
Guide to Low-Pressure Foaming Machines for PU Elastomers
Fully Automatic PU Shoe Production Line Explained
Maintenance Guide for Tire Foam Filling Machines
PU Foam Injection Machine: Key Components & Calibration Best Practices

Related Posts